Engineering plastics science - POM injection molding

release time:2024-01-08publisher:

POM injection molding process

1, plastic treatment

POM has low water absorption, generally 0.2%-0.5%. Under normal circumstances, POM can be processed without drying, but wet raw materials must be dried. The drying temperature is above 80℃ and the time is more than 2 hours, which should be carried out according to the supplier's information.

2, the selection of plastic machine

POM In addition to requiring the screw to have no hysteresis area, there is no special requirement for the injection molding machine, and the general injection molding can be done.

3. Mold and gate design

Common mold temperature control is 80-90℃, the diameter of the runner is 3-6mm, the length of the gate is 0.5mm, the size of the gate depends on the thickness of the rubber wall, the diameter of the circular gate should be at least 0.5-0.6 times the thickness of the product, the width of the rectangular gate is usually 2 times or more than the thickness, the depth is 0.6 times the wall thickness, and the release inclination is between 40 '-130'.

4, melting speed

POM-H can be set to 215℃ (190℃-230℃)

POM-K can be set to 205℃ (190℃-210℃)

5. Injection speed

The common speed is medium fast, too slow is easy to produce ripples, too fast is easy to produce jet and shear overheating.

6. Back pressure

The lower the better, generally no more than 200bar.

7. Retention time

If the equipment has no glue retention point,POM-H can be retained at 215 ° C for 35 minutes; POM-K can be retained at 205 ° C for 20 minutes without serious decomposition, and the melt cannot be retained in the barrel for more than 20 minutes at injection molding temperatures. POM-K can be retained for 7 minutes at 240℃. If the machine is stopped, the barrel temperature can be reduced to 150 ° C, if you want to stop for a long time, you must clean the machine cylinder and turn off the heater.

8. Stop

Cleaning the barrel must use PE or PP, turn off the electric heat, and push the screw in the front position. Barrel and screw must be kept clean. Impurities or dirt can change the overheating stability of POM (especially POM-H). Therefore, when the halogen-containing polymer or other acidic polymers are used, the POM material can be played after the PE is cleaned up, otherwise there will be an explosion. Improper use of pigments, lubricants or materials containing GF nylon can lead to plastic degradation.

9. Post-processing

For very warm parts and high quality requirements, heat treatment must be carried out. Annealing treatment effect, the product can be immersed in 30% hydrochloric acid solution for 30 minutes to check, and then use the naked eye to determine whether there is a residual stress crack.

Guangzhou Best Rubber & Plastic Co., Ltd. has more than 20 years of experience in POM injection molding, with more than 2,000 square meters of physical processing plants, but also has professional production and processing equipment, as well as professional design team, can provide customers with satisfactory products and services.

07.jpg

POM materials used in injection moulds

1. Steel

Commonly used steels are SKD11, DC53, etc. These steels have the characteristics of high hardness, high strength, good wear resistance, etc., which are suitable for making high-precision and high-demand molds.

2. Aluminum alloy

Aluminum table gold has the characteristics of light weight, corrosion resistance, good thermal conductivity, etc., and is widely used in some molds requiring low precision.

3. Cemented carbide

Cemented carbide has the characteristics of high hardness, high strength, good wear resistance, etc., which is suitable for making molds requiring high precision and high strength.

4. Polyimide (P1)

P1 has good high temperature stability and chemical corrosion resistance, suitable for making high temperature and high pressure molds.

5. Carbon fiber composite materials

Carbon fiber composite material has light weight, high strength, rigidity and good waiting point, which is suitable for making high-precision and high-demand molds.

24.jpg

POM injection molding precautions

1. Injection temperature

Under the circumstances, when the injection temperature is 20~30℃ higher than the melting point, not only the comprehensive physical and mechanical properties are good, but also the apparent smooth and flat products can be obtained at this temperature, so the injection temperature is controlled between 190~ 200℃. For thin-walled products, it can be increased to 210℃ for processing, exceeding this temperature not only can not improve the flow of the material, but may lead to the decomposition of the material.

2. Injection pressure

The injection pressure of POM plastic is related to the wall thickness of the product and the type of equipment. In order to ensure smooth demoulding, the injection pressure should not be too high.

3. Injection speed

The injection speed is slow, there will be poor welding. Thin-walled products are selected for rapid injection.

4. Mold temperature

Mold temperature is controlled at about 60~100℃.

5. Precautions

The production should be carried out continuously. If it is stopped, the residual material in the cylinder should be emptied to avoid material decomposition and product black spots when it is heated again. The molding temperature of POM is not allowed to exceed 240 ° C, at which temperature the material will quickly decompose. The material should not stay in the barrel above 190 ° C for too long, otherwise it will also cause the material to decompose. In the case of ensuring product quality and melt fluidity, lower molding temperature and shorter molding cycle should be selected as far as possible. The post-treatment of POM products is carried out with air or oil as the medium. The temperature is 140~150℃ and the time is 3~5h.

31.jpg

POM injection molding size fluctuation solution

1. The fluctuation of barrel temperature causes the change of product structure size. The barrel temperature should be stabilized.

2. The size fluctuation caused by the fluctuation of buffer quantity. The buffer should be kept constant.

3. Too low or too high mold temperature will lead to size fluctuations. Mold temperature should be controlled accurately.

4. The injection speed is too slow. The mold should be filled quickly.

5. Product cooling is not uniform, causing size instability. The products after demoulding should be treated by annealing process, and the products should still be uniformly cooled after demoulding.

6. Improper mold design. For multi-cavity mold, cavity arrangement form and gate size should be reasonably designed to ensure synchronous mold filling.


Title

Guangzhou?Best?Rubber?And?Plastic?Co.,Ltd.

  • Tel:(020)31523725, 31523097,15813393170
  • Fax:(020)37403270, 37403280
  • Email: sales@gz-best.com/export@gz-best.com
  • Add:No. 21 Liangtian Middle Road, Baiyun District, Guangzhou City, Guangdong Province
  • Add:25-27 Yanling Road, Guangzhou
久久综合中文字幕_肉丝袜脚交视频一区二区_91成人免费网站_性做久久久久久久免费看_一区二区三区在线视频观看_欧美精品自拍偷拍_极品美女销魂一区二区三区_亚洲欧美国产高清_欧美日韩高清一区二区_成人av一区二区三区_久久久亚洲欧洲日产国码αv_麻豆成人免费电影_欧美精品乱人伦久久久久久_国产精品网曝门_中文字幕在线播放不卡一区_国产精品久久99
成人av综合在线| 成人午夜大片免费观看| 国内精品国产成人国产三级粉色| 成人av中文字幕| 日韩视频在线一区二区| 亚洲一区二区三区四区不卡| 从欧美一区二区三区| 精品国产免费一区二区三区香蕉| 国产欧美一区二区三区沐欲| 一区二区三区在线不卡| 成人18视频在线播放| www日韩大片| 天天爽夜夜爽夜夜爽精品视频| 色综合天天综合网天天狠天天 | 欧美精品在线观看一区二区| 亚洲欧美日韩中文字幕一区二区三区| 国产成人精品午夜视频免费| 精品毛片乱码1区2区3区| 天堂va蜜桃一区二区三区| 91麻豆成人久久精品二区三区| 国产精品伦一区二区三级视频| 国产一区二区三区四| 欧美大片一区二区三区| 日韩专区欧美专区| 91精品国产综合久久蜜臀| 日韩综合一区二区| 91精品国产欧美一区二区| 日韩影院免费视频| 91麻豆精品国产91久久久久久| 亚洲一区二区不卡免费| 日本道色综合久久| 一区二区三区久久| 欧美网站一区二区| 天天综合天天做天天综合| 777xxx欧美| 蜜桃免费网站一区二区三区| 日韩女优视频免费观看| 激情av综合网| 国产亚洲精品aa| 成人h精品动漫一区二区三区| 国产精品久久久久7777按摩| 91色乱码一区二区三区| 一区二区三区四区乱视频| 91国偷自产一区二区开放时间| 亚洲一区免费在线观看| 欧美精三区欧美精三区| 麻豆精品在线观看| 久久久久久麻豆| 成人综合婷婷国产精品久久| 国产精品久久久久久久久久久免费看 | 久久久亚洲午夜电影| 国产精品99久| 中文子幕无线码一区tr| 99久久伊人网影院| 亚洲综合精品自拍| 亚洲va欧美va人人爽| 欧美一区二区三区小说| 久久66热偷产精品| 亚洲国产高清在线| 色婷婷一区二区| 日韩精品国产精品| 久久综合色之久久综合| av资源站一区| 亚洲无线码一区二区三区| 欧美一区二区三区免费观看视频| 国内精品久久久久影院色 | 国产一区二区三区av电影| 国产欧美1区2区3区| 一本一道久久a久久精品综合蜜臀| 亚洲成人自拍网| 精品裸体舞一区二区三区| 成人污视频在线观看| 夜夜嗨av一区二区三区中文字幕| 91精品国产91热久久久做人人 | 色噜噜狠狠成人中文综合| 亚洲va中文字幕| 精品成人佐山爱一区二区| gogogo免费视频观看亚洲一| 五月天激情综合网| 国产亚洲精品资源在线26u| 色婷婷av一区二区三区gif| 免费黄网站欧美| 国产精品久久久久久久第一福利 | 亚洲永久精品国产| 日韩精品一区二区三区视频在线观看 | 国产欧美日韩在线视频| 在线亚洲人成电影网站色www| 免费成人性网站| 亚洲欧洲日产国码二区| 这里只有精品视频在线观看| 国产999精品久久| 亚洲成av人影院| 欧美国产精品久久| 在线播放亚洲一区| 99久久精品国产麻豆演员表| 日韩高清在线不卡| 中文字幕日韩一区| 欧美一级生活片| 95精品视频在线| 韩国女主播成人在线观看| 亚洲精品免费在线| 久久婷婷国产综合国色天香| 欧美日韩一级视频| 不卡一区二区在线| 另类综合日韩欧美亚洲| 一区二区成人在线视频| 国产亚洲1区2区3区| 欧美日韩国产另类不卡| 不卡av在线网| 国内欧美视频一区二区| 亚洲第一主播视频| **欧美大码日韩| 久久久久国产精品厨房| 欧美日产国产精品| 色悠悠久久综合| 国产91对白在线观看九色| 午夜精品福利一区二区三区av| 国产精品美女久久久久久| 精品国产一区a| 911精品国产一区二区在线| 91看片淫黄大片一级在线观看| 国产在线视频一区二区| 日韩精品三区四区| 一区av在线播放| 日韩毛片在线免费观看| 久久久无码精品亚洲日韩按摩| 欧美裸体一区二区三区| 中文字幕一区二区三区在线观看| 欧美一区午夜视频在线观看| 91福利区一区二区三区| 成人激情免费电影网址| 国产精品911| 精品一区二区三区日韩| 日本在线不卡视频| 亚洲国产成人高清精品| 亚洲人妖av一区二区| 中文字幕巨乱亚洲| 国产亚洲精品bt天堂精选| 精品国产91久久久久久久妲己 | 中文字幕一区二区三区在线不卡 | 天堂va蜜桃一区二区三区漫画版| 亚洲精品免费电影| 亚洲欧洲另类国产综合| 国产欧美一区二区三区沐欲| 久久品道一品道久久精品| 欧美一区2区视频在线观看| 欧美麻豆精品久久久久久| 欧美视频三区在线播放| 色噜噜久久综合| 91免费观看在线| 99久久国产综合精品女不卡| 成人黄色a**站在线观看| 成人美女视频在线看| 国产成人精品免费| 国产精品一二三四五| 韩国理伦片一区二区三区在线播放| 美女精品一区二区| 蜜臀91精品一区二区三区 | 成人av先锋影音| 成人动漫av在线| 99久久免费视频.com| 99国产精品视频免费观看| 不卡的av网站| 91在线观看一区二区| 91色乱码一区二区三区| 91福利在线导航| 欧美久久一二区| 日韩视频免费直播| 26uuu欧美| 国产欧美日韩在线| 国产精品不卡一区| 亚洲激情第一区| 香蕉成人啪国产精品视频综合网| 亚洲 欧美综合在线网络| 亚洲不卡av一区二区三区| 日本女优在线视频一区二区| 美女网站色91| 国产一区二区视频在线播放| 国产成人精品综合在线观看 | 欧美日韩一区中文字幕| 欧美久久久一区| 欧美成人bangbros| 久久久精品免费网站| 国产精品久久久久婷婷| 亚洲人成影院在线观看| 亚洲国产成人av网| 麻豆专区一区二区三区四区五区| 国产乱淫av一区二区三区| 成人午夜av电影| 在线中文字幕一区| 在线播放日韩导航| 久久免费视频一区| 国产精品传媒入口麻豆| 亚洲成人午夜电影| 毛片av一区二区| 成人免费观看视频| 欧美视频一区二区| 精品久久久三级丝袜| 国产精品国产三级国产有无不卡| 亚洲资源在线观看|